Electrolyte ready for use for selective decorative pencil gold-plating (brush gold-plating). The metal is deposited by means of a wiping touch with a soaked brush. Works at room temperature.
| Metal content in the deposit wt.% | Alloy compo- nents | Hardness of deposit HV 0.025 (Vickers) approx. values | Colour of deposit | Max. coating thickness μm |
Metal content g/l | pH- value | Voltage |
Plating speed μm/min approx. values | Tempe- rature °C |
| 99.5 | Diffe- rent | - | Rich deep yellow, fine gold colour |
0.1 | 20 | 7.0 | 10 V (8-15 V) | 0.1 | 20-30 |