Coatings with good corrosion and abrasion resistance as well as high hardness. For rack and barrel. Often used for bathroom fittings.
| Metal content in the deposit wt.% | Alloy compo- nents | Hardness of deposit HV 0.025 (Vickers) approx. values | Colour of deposit | Max. coating thickness μm |
Metal content g/l | pH- value | Current density A/dm2 |
Plating speed μm/min approx. values | Tempe- rature °C |
| 96.5 | Ni/In | 270 | 14 ct Hamilton (pale yellow) | 5 | 4 (3.5-4.5) | 3.5 (3.4-3.7) | 0.6 | 0.06 | 30 (28-32) |