Coatings with stable colour, good corrosion and abrasion resistance as well as high hardness. For rack and barrel. Hot-water post-treatment is recommended. Specially for the bath- room fittings industry.
| Metal content in the deposit wt.% | Alloy compo- nents | Hardness of deposit HV 0.025 (Vickers) approx. values | Colour of deposit | Max. coating thickness μm |
Metal content g/l | pH- value | Current density A/dm2 |
Plating speed μm/min approx. values | Tempe- rature °C |
| 92.5 | Ni/Co | 290 | Yellow-grey | 1 | 2.5 (2-3) | 4.0 (3.8-4.2) | 1.0 | 0.12 | 50 (48-52) |