GOLD IRON INDIUM ELECTROLYTE

AURUNA® 215 is a colour gold alloy electrolyte for decorative applications, preferably for parts coming into contact with the skin such as jewellery and watches. The essential advantage of the coatings is their freedom from nickel and cobalt, excluding skin allergies caused by these metals. The weakly acidic gold electrolyte is easy to operate and suitable for rack and barrel, it works very colour-constant. Across a wide operating range, the coating colour (1N - 2N) is independent of pH-value and current density. By adding indium, a uniform colour is achieved.

Advantages
• Weakly acidic colour gold electrolyte
• Pale to light yellow coatings
• Colour-constant across a wide operating range
• Uniform colour
• For decorative applications
• Non-allergenic since free of nickel and cobalt
• The coatings are RoHS compliant
• Suitable for rack and barrel

Applications
• Jewellery
• Watches
• Spectacle frames
• Writing implements
• Accessories




ELECTROLYTE CHARACTERISTICS

 

 


COATING CHARACTERISTICS

 

  Electrolyte type

Weakly acidic

 

Coating

Gold-iron-indium

 Metal content

2.5 (2.0 - 3.0) g/l Au0.5 (0.4 - 0.6) g/l Fe
1.0 (0.8 - 1.2) g/l In

 

Alloy composition

98.5 weight % Au1.4 weight % Fe
0.05 weight % In

pH value

4.0 (3.8 - 4.5)

 

Colour of deposit

Approx. 1N - 2N

Operating temperature

35 (30 - 35) °C

 

Brightness

Bright

Current density range

1.5 (0.5 - 2.0) A/dm²

 

Hardness of deposit
HV 0.015 (Vickers)
approx. values

220 HV

Plating speed

Approx. 0.14 μm/
min at 1.5 A/dm²

 

Max. coating thickness

3 μm

Anode material

Pt-Ti, MMO (type PLATINODE    147)

 

Density of the coating

Approx. 17.5 g/cm³

     