Electrolyte ready for use for selective decorative pencil rhodium-plating (brush rhodium-plating). Abrasion-resistant, light and bright coatings. High plating speed, fast covering. 

Metal content in the deposit wt.%  Alloy compo- nents  Hardness of deposit HV 0.025 (Vickers) approx. values  Colour of deposit  Max. coating  thickness
μm 
Metal  content g/l pH- value  Voltage  Plating speed μm/min approx. values  Tempe-  rature °C 
99.9  800  White  Up to 1  20  <1  8-10 V (max. 12 V )  Up to 0.2  20-40