Gold-saving, approx. 12 carat gold-silver coatings. Mainly used for gold-saving intermediate layers under final layers of higher caratage. Resistant to corrosion and tarnishing. Excellent ductility, no cracking when bent. For rack and barrel.
Metal content in the deposit wt.%
Alloy compo- nents
Hardness of deposit HV 0.025 (Vickers) approx. values
Colour of deposit
Max. coating thickness μm
Metal content g/l
pH- value
Current density A/dm2
Plating speed μm/min approx. values
Tempe- rature °C
50
Ag
220 HV 0.015
Yellowish white
20
6 (5-6)
0.6-0.8
0.5 (0.3-0.8)
0.3-0.45
45 (40-47)